SYUDOX® PRF series & PR-30RS
Waterproofing Agents [Powder]
SYUDOX® PRF series and SYUDOX® PR-30RS are the powder type waterproofing agents for the addition in construction site or premixed products.
✔Having little impact on the workability.
✔Easy to mix with other power.
| 
 Item  | 
 SYUDOX® PRF-C180  | 
 SYUDOX® PRF-A180  | 
 SYUDOX® PR-30RS  | 
| 
 Appearance  | 
 White powder  | 
 White powder  | 
 White powder  | 
Depending on the application, the dosage of SYUDOXPRF®Series, and PR-30RS varies from 1.0 to 3.0wt% of the cementitious material.
PRF-C180 : 0.5 ~ 2.0 wt% (vs. Cement)
PRF-A180 : 0.5 ~ 2.0 wt% (vs. Cement)
Table 1. Mixture proportion of the mortar
| 
 W/C [%]  | 
 S/C  | 
 Redispersible polymer powder dosage [C×%]  | 
 Defoaming agent dosage [C×%]  | 
| 
 50.0  | 
 2.0  | 
 5.0  | 
 1.0-2.0  | 
W: Water C : Ordinary portland cement S : Fine aggregate (Silica sand) Redispersible polymer powder: acryl type

Figure 1.Relationship between waterproofing agents dosage and 24h water absorption ratio.
Table 2.Influence of waterproofing agent to mortar property (at 22±2℃)
| 
 Waterproofing agent  | 
 Dosage [C×%]  | 
 Unit weight [g/L]  | 
 Mortar flow [mm]  | 
 Strength [N/mm2]  | 
|
| 
 Flexural  | 
 Compressive  | 
||||
| 
 28days  | 
 28days  | 
||||
| 
 Control①*1)  | 
 -  | 
 2,070  | 
 167  | 
 9.6  | 
 34.8  | 
| 
 Control②*2)  | 
 -  | 
 2,070  | 
 168  | 
 10.2  | 
 39.1  | 
| 
 SYUDOX® PRF-C180  | 
 1.0  | 
 1,970  | 
 165  | 
 -  | 
 -  | 
| 
 2.0  | 
 1,920  | 
 162  | 
 8.9  | 
 28.7  | 
|
| 
 SYUDOX® PRF-A180  | 
 1.0  | 
 2,040  | 
 164  | 
 -  | 
 -  | 
| 
 2.0  | 
 2,030  | 
 162  | 
 9.9  | 
 28.8  | 
|
| 
 SYUDOX® PR-30RS  | 
 1.0  | 
 2,000  | 
 166  | 
 -  | 
 -  | 
| 
 2.0  | 
 1,950  | 
 162  | 
 7.8  | 
 29.1  | 
|
*1) Control① : No redispersible polymer powder *2) Control② : Only redispersible polymer powder
Figure 2.Relationship between waterproofing agents dosage and 24h water absorption ratio.

Control SYUDOX® PR-30RS
PRF-C180   :   0.5 ~ 2.0 wt% (vs. Cement)
PRF-A180   :   0.5 ~ 2.0 wt% (vs. Cement)
(1) Mixing Proportion

(2) Testing condition
① The test pieces were molded in 40×40×160mm prisms and were demolded after 24 hours,
    cured in air until the age of 3 days and kept in a room with a temperature of 20℃ or 80℃.
② The base weight of the test piece was measured at the age of 3days.
③ The test pieces were cured in water for 24 hours
④ The weight of the test piece was measured. 
    Absorption(%) = [ (④weight) - (②weight) ] / (②weight) × 100
(3) Results

| HANDLING | : Avoid contact with eyes. Avoid prolonged or repeated contact with skin.When handling at elevated temperature, provide adequate ventilation. Avoid rough handling or dropping. | 
| FIRST AID MEASURES | |
| EYE | : Immediately flush with clean water until irritation disappear sufficiently, and consult a physician if necessary. | 
| SKIN | : Immediately wash thoroughly with plenty of water. | 
| INGESTION | : Immediately induce vomiting, and rinse mouth with water. If symptoms are not good after first-aid measures, consult a physician immediately. Do not induce vomiting or give anything by mouth to an unconscious parson. | 
10 KGS NET IN A PAPER SACK
- Best fit dosage of PRF series depends on aggregate, mortar temperature and so on, try premix to give objective mortar.
 - To the best of our knowledge, although certain hazards are described herein, we cannot guarantee that these are the only hazards which exist.
 